Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Ultrason E - PESU - BASF

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Ultrason E" in Material Data Center leads to the following information:

Tradename: Ultrason E
Family: PESU
Producer: BASF
20 hits in the material database
7 hits in the literature database
13 hits in the application database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Application
Ultrason E Housing, cartridges, inkjet printer
Ultrason E Trip switch, functional parts
Ultrason E Headlight system
Ultrason E Headlight-reflector
Ultrason E Housing, fog lights
Ultrason® E 2010 HC Visor, firefighter's helmet
Ultrason® E 2020 P Coupling agent, non-stick layer of coated pans
Ultrason® E 6020 P Membrane filter
Ultrason® E 6020 P Hollow fiber, water purification system
Ultrason E 2010 C2 TR Oil pump piston
Ultrason® E 2010 MR Reflector, interior lighting
Ultrason E Switch latches, fuse holders and circuit breaker covers
Ultrason® E 2010 C6 Sandwich structures for airplane interiors

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.